An epoxidized natural rubber (ENR) blend with chlorhexidine gluconate (CHG) was prepared using a two-roll mill at 130 °C. CHG was added at concentrations of 0.2, 0.5, 1, 2, 5, and 10% (w/w) as an antimicrobial additive. The ENR blend with 10% (w/w) CHG showed the best tensile strength, elastic recovery, and Shore A hardness. The ENR/CHG blend exhibited a smooth fracture surface. The appearance of a new peak in the Fourier transform infrared spectrum confirmed that the amino groups of CHG reacted with the epoxy groups of ENR. The ENR with 10% CHG exhibited an inhibition zone against Staphylococcus aureus. The proposed blending improved the mechanical properties, elasticity, morphology, and antimicrobial properties of the ENR.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.