ObjectiveTo investigate whether proanthocyanidins (PA) is capable of improving dentin collagen's biological stability through cross-linking within time periods that are clinically relevant. Materials and methodsDemineralized dentin collagen slabs were treated with 3.75wt% PA solution for 10s, 1min, 30min, 60min, 120min, 360min, and 720min, respectively. The resultant cross-linked collagen samples were subject to digestion with 0.1% collagenase at 37°C for 2h, 6h, 12h, 24h, 36h, and 48h. The percentage of weight loss after digestion was calculated to evaluate PA-treated collagen's resistance toward enzymatic degradation. Fourier-transformed infrared (FTIR) spectroscopy was used to probe evidences of PA-collagen interactions after various periods of PA treatment. ResultsThe collagenase digestion assay suggests that PA treatment as short as 10s can enhance collagen's resistance toward enzymatic challenge. The FTIR spectroscopy further verifies that PA is indeed incorporated into collagen regardless of treatment time, possibly via a mechanism involving the chemical interactions between PA and collagen. SignificanceThis study confirmed that PA can effectively cross-link collagen and improve its biological stability in time periods as short as 10s. The use of PA as a priming agent is therefore clinically feasible and is a promising approach to improving the durability of current dentin bonding systems.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.