Abstract

To improve the thermoelectric properties of Ce–doped Bi2Sr2Co2Oy, the structural and thermoelectric properties of Bi2–xCexSr2Co2Oy (0 ≤ x ≤ 0.15) prepared by both conventional sintering (CS) and spark plasma sintering (SPS) are investigated. As the Ce concentration in the CS processed Bi2–xCexSr2Co2Oy samples increases, the electrical conductivity decreases and the Seebeck coefficient and thermal conductivity increase. On the other hand, the electrical conductivity, Seebeck coefficient, and thermal conductivity of the SPS processed Bi2–xCexSr2Co2Oy samples increase with increasing Ce concentration. The SPS processed samples show a significantly larger dimensionless figure−of−merit ZT compared to the CS processed samples due to the larger electrical conductivity and Seebeck coefficient. The high-est dimensionless ZT (0.13) at 973 K is achieved for the SPS processed Bi1.85Ce0.15Sr2Co2Oy. This ZT is nearly three times larger than that of the CS processed Bi2Sr2Co2Oy (0.045) at 973 K. Our results indicate that the SPS and Ce doping are highly effective strategies for improving the thermoelectric properties of Bi2Sr2Co2Oy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.