Abstract

Austempering is conducted below and above martensite start temperature (Ms) at the fine and coarse prior austenite grain size (PAGS), respectively, in a low‐carbon bainitic steel, and the relationship between multiphase microstructure and mechanical properties is investigated. The study indicates that refinement of bainite laths can be obtained by decreasing the PAGS and/or austempering temperature from above to below Ms. The former reduces bainite content, and increases the volume fraction of retained austenite (RA), thereby obtaining higher uniform elongation and strain hardening exponent. However, the latter effectively decreases the size and amount of blocky RA, as well as bainite content and conversely increases the ratio of volume fraction of film RA to that of blocky RA, which leads to significant improvement in yield strength and impact toughness. In addition, the variant selection is relatively weak with the decrease in the PAGS and austempering temperature, which has a beneficial effect on toughness. Furthermore, an outstanding combination of mechanical properties (1070 MPa yield strength, 1466 MPa tensile strength, total elongation of 11.68%, and V‐notch impact toughness at 20 and −40 °C of 78 and 44 J cm−2, respectively) is achieved by austempering below Ms in the finer PAGS.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.