ABSTRACTBeneficiation of low-grade iron ore was carried out by selective flocculation process using different flocculants, namely starch amylopectin (AP) and grafted copolymer of amylopectin (GAP). The iron ore used in the investigation contained 56.98% Fe, 5.45% Al2O3, and 4.22% SiO2. Flocculant dosage, number of floc washing, and pH were considered as variable parameters to analyze their effect on the performance of grade and recovery of concentrate. A flocculant dosage of 0.4 mg/g was found to be the optimum condition for the sample and variable parameters under investigation. The investigation indicated that a grade of 64.77% Fe can be obtained with 96% recovery using AP; however, GAP showed the better result for Fe grade (67%) with a recovery of 97%.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.