Abstract

In this study, we achieved an enhanced d33 of 350–400 pC N−1 in the dense 0.96(K0.4Na0.6)(Nb0.96Sb0.04)O3–0.04Bi0.5K0.5Zr0.9Sn0.1O3 ceramics over a wide sintering temperature range of 400–1050 °C by two-step sintering.