Abstract

Abstract. The effect of Au, Ag & Cu (1 wt%) photodeposition onto CdS nanorod (length ~ 116 nm, aspect ratio = 21, surface area = 81 m2/gm) has been studied by photocatalytic degradation of 0.5 mM salicylic acid both under direct sunlight and UV (125 W Hg arc lamp, 10.4 mW/cm2) irradiation. The bare CdS nanorod (NR) exhibited higher photoactivity as compared to low activity of bare CdS (~10 nm) nanosphere (NS) and Au & Ag photodeposition highly improved the CdS nanorod photoactivity compared with Cu deposition. The fluorescence emission of CdS nanorod at 479 nm is also quenched due to metals deposition. It is observed that Au-CdS (20 mg) nanorod composites completely degrade 0.5 mM (20 ml) salicylic acid within 2 h sun light exposure. The significant effect of Au-CdS photocatalytic activity on the various sizes (3.5 & 2 nm) of Au deposits has been observed during salicylic acid photodegradation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.