Abstract

We report the enhanced tensile strength and creep resistance of a new Ni–Co-base superalloy (TMW-2) by increasing the solution temperature from 1100 °C to 1140 °C. The yield strength could be improved by 60 MPa, and a temperature gain in creep resistance of about 15 °C could be achieved. The improvements in yield strength and creep resistance are mainly due to the coarsening of grain size, the increasing of the volume fraction of tertiary γ′ and of the length of annealing twin formed during the heat treatment.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.