Abstract

Using B4C and C additives, a HfB2–SiC composite with an enhanced strength up to 1600 °C was prepared using high-energy ball milling followed by hot pressing. The composite microstructure comprised equiaxed large HfB2 and fine SiC grains and an intergranular amorphous phase. The mechanical behaviour of the composite was evaluated up to 1600 °C via a four-point bending test. At or below 1500 °C, only a linear stress–strain response was observed. At 1600 °C, however, the initial linear response was followed by nonlinear deformation behaviour. The flexural strength was constant between room temperature and 1400 °C; subsequently, the flexural strength significantly increased with increasing temperature up to 1600 °C, with strengths in the range of 650–750 MPa.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.