Abstract
Ni-based cathode materials have been as an alternative to LiCoO2[1,2]. Therefore, many studies have been performed to solve the inherent problems of Ni-base cathode materials [3]. However, reasonable solution for rate performance and thermal stability of Ni-based cathode materials has not been reported. Coating method on the cathode material may become the solution technique for electrochemical properties. In this study, LiNi0.5Co0.2Mn0.3O2 cathode materials were prepared by co-precipitation method. RuO2 coating layer was deposited on LiNi0.5Co0.2Mn0.3O2powder using a shower head type PEALD reactor (Lucida-M100, NCD Technology), with IMBCH Ru [IMBCH = (η6-1-isopropyl-4-methylbenzene)(η4-cyclohexa-1,3-diene)] as a precursor. We propose a new coating method for cathode materials using atomic layer deposition. The physical and electrochemical properties of RuO2 coated LiNi0.5Co0.2Mn0.3O2 cathode materials have been thoroughly investigated. Compared to various metal oxides, we will show that the optimization of RuO2 coating layer can be significantly improved the electrochemical performance of LiNi0.5Co0.2Mn0.3O2cathode materials.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.