Very high electrical conductivity of ∼0.021 S/cm at 600 °C is obtained in Ce 0.79Gd 0.20Co 0.01O 2− δ . Corresponding activation energy of conduction ∼0.43 eV measured in the temperature range of 400–700 °C is found to be notably low. Improved electrical properties with 99% of the theoretical density as obtained for these specimens, prepared using powder of average particle size ∼20 nm and subsequent sintering at 1100 °C, is considered to be a significant step to reduce the processing temperature. The measured electrical potential of ∼1 V indicates the suitability of its use as an electrolyte in electrochemical devices.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.