Abstract

Silicon oxide (SiO x ) thin film was deposited onto poly(ethylene terephthalate) substrate by the reduction of an aqueous solution containing ammonium hexafluorosilicate, dimethylamine borane and cetyltrimethylammonium bromide (CTAB). Post-deposition hot water treatment: immersion of the film in water at 333 K dissolved CTAB producing nanopores in silica (SiO 2) film and remarkably enhanced the antireflection property of the film: 0.1% at 550 nm of wavelength. The films before and after the treatment were compared via characterization by means of X-ray photoelectron spectroscopic depth profile, X-ray diffraction and transmission electron microscopy. The decrease of refractive index dispersion by the porous silica films, attributing to the low reflection, was verified by effective medium approximation analysis.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.