A study was carried out to compare the ballistic performance of high purity alumina and zirconia-toughened alumina (ZTA) using depth of penetration (DoP) test configuration against 7.62 mm armour piercing (AP) ammunition. The effect of tile thickness on the differential efficiency factor (DEF) was studied for tile thickness in the range of 3 mm to 6 mm for alumina tiles and 3 mm to 5 mm for ZTA tiles. The DEF is found to increase as tile thickness increases. An analysis on the failed shots showed that the residual shot weight does not follow a single linear relationship with ceramic tile thickness unlike the residual DoP for all thicknesses of tiles. Post-ballistic analysis on ceramic powder for particle size distribution was carried out and the results are presented. Defence Science Journal, Vol. 64, No. 5, September 2014, pp.477-483, DOI:http://dx.doi.org/10.14429/dsj.64.6745