Abstract

Converting waste coal combustion ash (W-CCA) from power plants into novelty lightweight aggregates (LWA) is a viable and sustainable solution. Utilizing this waste material to produce a useful product for the concrete industry requires that the manufactured LWA adhere to industrial material regulations. This study focuses on engineering laboratory manufactured LWA to achieve aggregate gradation that meets the ASTM C330 standard. A systematic study that manipulates the degree of saturation during W-CCA paste preparation was adopted to understand the effect of moisture on LWA gradation. The degree of saturation was assessed based on the liquid (water) to solid ratio required to manufacture W-CCA paste. The investigation only alters the amount of water and recorded the gradation for fine LWA (FLWA), coarse LWA (CLWA), and combined coarse and fine LWA. L/S ratio of 0.33 achieved ASTM C330 required gradation for FLWA. A combination of L/S ratio of 0.33 and 0.34 achieved ASTM C330 required gradation for combined coarse and fine LWA. Engineering the gradation of LWA to meet ASTM required standard will allow the production of LWA from W-CCA a more attainable and practical product for the construction industry.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.