Great efforts have been made to understand and upgrade the kinetically sluggish oxygen evolution reaction (OER). In this study, a series of V-doped LaCoO3 (V-LCO) OER electrocatalysts with optimized d-band centers are fabricated. When utilized as an electrode for the OER, as-formed LaCo0.8 V0.2 O3 (V-LCO-II) requires an overpotential of only 306 mV to drive a geometrical catalytic current density of 10 mA cm-2 . Furthermore, at a given overpotential of 350 mV, the OER current density of V-LCO-II is about 22 times that of pure LaCoO3 (LCO) nanoparticles. Tailoring of the d-band center by V doping facilitates the adsorption of OER intermediates and promotes the formation of amorphous active species on the surface of LCO through the exchange interaction between high-spin V4+ and low-spin Co2+ . This work may create new opportunities for developing other highly active OER catalysts through d-band center engineering.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.