The photoluminescence properties and energy transfer of a new Ce3+/Pr3+/Eu3+ co-doped solid-solution composition of Sr2.975−xLaxAlO4+xF1−x (LSAF) phosphor are investigated. Upon doping Pr3+ into lattices of LSAF:Ce host, a shoulder emission peak is observed at about 620 nm, owing to the transition of 1D2 → 3H4. Addition of Eu3+ to LSAF:Ce3+, Pr3+ phosphor results in a sharp emission peaked at 675 nm for the 5D0 → 7F3 transition and an increase of the intensity of red emission for Pr3+ with increasing Eu3+ concentration. The pathways of energy transfer among Ce3+, Pr3+, and Eu3+ are proposed to be responsible for color addition of a red component to the primary yellow emission, enabling a potential adjustable color for blue excitable warm white.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.