Abstract

Series of Sr2MgAl22O36:Ce3+, Sr2MgAl22O36:Dy3+ and Sr2MgAl22O36:Ce3+,Dy3+ phosphors were synthesized by urea-assisted combustion method. The identification of phase and morphology of the prepared samples were characterized by X-ray diffraction (XRD) and scanning electron microscopy (SEM). Photoluminescence excitation (PLE) and emission spectra of the as-prepared samples were investigated. Photoluminescence studies revealed that the luminescence intensity of Ce3+ ion increases with increasing concentration in Sr2MgAl22O36:Ce3+ and no concentration quenching have been witnessed. Similar trend was observed for Sr2MgAl22O36:Dy3+ with increasing Dy3+ concentration. The energy transfer from Ce3+ to Dy3+ in Sr2MgAl22O36 host has been achieved successfully to produce white light emission. The calculated Commission Internationale de L′Eclairage (CIE) chromaticity coordinates for the Sr2MgAl22O36:Ce3+, Dy3+ phosphor are (x = 0.302, y = 0.357). The values of CIE chromaticity coordinates and correlated color temperature (CCT) of 6798 K endorse Sr2MgAl22O36:Ce3+, Dy3+ phosphor as potential candidate for cool white-light emission.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.