The preparation of nanostructured ZnAl 2O 4 spinel powders doped with Eu 3+ ions obtained by a hydrothermal method is described. XRD analyses demonstrated that the powders were single-phase spinel nanopowders with high crystallite dispersion. The averaged spinel particle size was determined to be 6 nm as prepared and it increased up to 8 nm for calcination at 500°C. The emission spectra of Eu 3+ ions measured for the samples calcinated at 500°C demonstrated inhomogeneous shapes characteristic for disordered material which after heating at 1500°C changed shape into an ordered shape characteristic of the crystalline form.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.