Abstract

We study the chemical and structural inhomogeneities and the parameters of wear resistance of the coatings obtained by the arc-welding method. The coatings were obtained from PR-KhN80SSR3, PN-AN-34, and Kh17N8S6G powders based on nickel, cobalt, and iron, respectively, and from an experimental powder based on Ni and Fe. The tribological properties of iron-based alloys are better than for the cobalt- and nickel-based alloys. In the course of friction, the austenitic component of the coating undergoes plastic deformation as a result of which it covers the surface as a lubricant, which decreases the friction coefficient and wear.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.