Abstract

The effects of brazing time on elements diffusion and bonding strength of vacuum brazed joints of 15-5PH stainless steel using filler metal BNi-2 were investigated. The results showed that the brazing time determined the content of diffused elements. If holding time is short the distribution of melting point depressants (MPD) concentrated on the middle zone of the joint, and the generation of brittle phases in the joint was unavoidable. With increasing time, MPD can diffuse to base metal adequately and full solid solution of nickel formed in the brazing joint. Joint strength firstly increased and then decreased with prolonging holding time.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.