La3(BWO9):Tb3+ nanofibers were fabricated by an electrospinning process. The XRD patterns of the obtained fibers indicate that the incorporation of Tb3+ ions will not change the phase of La3(BWO9). The excitation spectrum monitored at 547 nm consists of excitation bands originating from 1T1 → 1A1 transition of O2− → W6+ in the WO6 group and 4f8 → 4f75d1/4f8 transitions of Tb3+. Upon the excitation at 362 nm, La3(BWO9):Tb3+ fibers show emission bands originating from the 5D4 → 7Fj (j = 6, 5, 4 and 3) transitions of Tb3+. The decay characteristics of La3BWO9:Tb3+nanofibers indicate that Tb3+ ions occupy one site in the host lattice.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Materials Science: Materials in Electronics
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.