Abstract

In the study, morphology, composition, and hardness of the coatings formed by electrospark alloying (ESA) of titanium with zirconium and subsequent induction heat treatment were considered. The possibility of forming coatings with a maximum size of oxide crystals of 8.9±3.8 μm and an open porosity reaching 58 % was established. The morphology parameters depend on the modes of electrospark alloying and heat treatment. There was a decrease in zirconium content in the coating composition from 21.9 to 1.1 at.% when the temperature and duration of induction treatment were increased. Maximum hardness equalled 10.3±0.3 GPa.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.