1. 1. With an increase in specific energy lower olefin yield and gas yield increse. 2. 2. With an increase in the temperature of heating of the raw material, ethylene, propylene, butane and divinyl contents and gas yield and, in resin, the content of aromatic hydrocarbons increase. 3. 3. A conducting material can be used as catalyst in pyrolyis. 4. 4. With a specific energy of 0·5 kWh/kg gasoline the extent of gas formation is 79% and ethylene content in the final gas (% wt.) is 31, propylene, 25, butanes and divinyl 13.