Abstract

The substantial promotion of hydrogen evolution reaction (HER) catalytic performance relies on the breakup of the Sabatier principle, which can be achieved by the alternation of the support and electronic metal support interaction (EMSI) is noticed. Due to the utilization of tungsten disulfides as support for platinum (Pt@WS2), surprisingly, Pt@WS2 demands only 31 mV overpotential to attain 10 mA cm‐2 in acidic HER test, corresponding to a 2.5‐fold higher mass activity than benchmarked Pt/C. The pH dependent electrochemical measurements associated with H2‐TPD and in‐situ Raman spectroscopy indicate a hydrogen spillover involved HER mechanism is confirmed. The WS2 support triggers a higher hydrogen binding strength for Pt leading to the increment in hydrogen concentration at Pt sites proved by upshifted d band center as well as lower Gibbs free energy of hydrogen, favourable for hydrogen spillover. Besides, the WS2 shows a comparably lower effect on Gibbs free energy for different Pt layers (‐0.50 eV layer‐1) than carbon black (‐0.88 eV layer‐1) contributing to a better Pt utilization. Also, the theoretical calculation suggests the hydrogen spillover occurs on the 3rd Pt layer in Pt@WS2; moreover, the energy barrier is lowered with increment in hydrogen coverage on Pt.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.