Abstract

The ZnO samples were prepared by firing at ∼900°C, finely powdered material under different degrees of reduction. Measurements of the green cathodoluminescence (CL) were done by using a vacuum fluorescent display. The g values of ESR spectrum measured from the powders at 77 K were g ‖ = 1.956±0.001 and g ⊥ = 1.955±0.001. The ESR signal of donors arises from the oxygen vacancy. The temperature dependence of line shapes and intensities of the center were investigated. The intensities of CL obtained were nearly inversely proportional to the intensity of ESR signal at g ⋍ 1.955 for various reducing conditions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.