The effects of amorphous SiO2 coating onto FeSiCr alloy powder on the electric and magnetic properties were investigated. FeSiCr alloy powder with an average particle size of 10 μm was coated with nano-sized silica powder to increase the resistivity and DC bias superposition characteristics. Inexpensive water glass (sodium silicate) was used as the raw material to form the amorphous silica layer onto the FeSiCr alloy powder surface acting as a binding and insulation layer. The amorphous silica layer thickness was about 20 nm to 50 nm. The thickness can be controlled by the amount of sodium silicate addition. The amorphous silica layer can significantly promote anti-oxidation, resistivity and DC bias superposition characteristic of the FeSiCr alloy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.