Abstract

In this study, the electrochemical treatment has been investigated in the real acidic effluent of copper-phthalocyanine dye manufacturing plant. Galvanostatic batch electrolyses have been carried out in an undivided cell using stainless steel as cathode, dimensionally stable anode (DSA) and graphite as anodes at different current densities and temperatures. The influence of these variables on current efficiency, cell voltage, energy consumption and deposit quality was reported. Under optimized conditions, the maximum copper recovery of 98% and COD removal efficiency of 87.3% with the energy consumption of about 11.23 kWh/kg of Cu and 6.08 kWh/kg of COD, respectively at 30 °C were achieved in the acidic raw effluent using 2D parallel-plate cathode. While in 3D stainless steel turning cathode reactor, 99.5% of copper can efficiently be recovered from dilute solution with an acceptable current efficiency of about 56.8% with minimum energy consumption of 2.37 kWh/kg of Cu. The experimental results suggested that the efficiency of copper removal is hindered by the presence of organic species in the mixed industrial effluent.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.