Abstract

The possibility of using hyperhigh speed high current electrodischarged Ti-plasma, generated by coaxial magnetoplasma accelerator as a method for Ti-C, Ti-B and Ti-Si coatings is shown. It is estimated that the most ordered microstructure is formed for a sample obtained under W = 46.7 kJ and 2.0 g carbon load. The average level of nanohardness for this sample is 15.3 GPa.