The growth of stoichiometric CuInSe(2) (CIS) on Au substrates using electrochemical atomic layer deposition (E-ALD) is reported here. Parameters for a ternary E-ALD cycle were investigated and included potentials, step sequence, solution compositions and timing. CIS was also grown by combining cycles for two binary compounds, InSe and Cu(2)Se, using a superlattice sequence. The formation, composition, and crystal structure of each are discussed. Stoichiometric CIS samples were formed using the superlattice sequence by performing 25 periods, each consisting of 3 cycles of InSe and 1 cycle of Cu(2)Se. The deposits were grown using 0.14, -0.7, and -0.65 V for Cu, In, and Se precursor solutions, respectively. XRD patterns displayed peaks consistent with the chalcopyrite phase of CIS, for the as-deposited samples, with the (112) reflection as the most prominent. AFM images of deposits suggested conformal deposition, when compared with corresponding image of the Au on glass substrate.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.