Abstract

AbstractElectrocopolymerization of a binary mixture of 3‐chloroaniline and 2‐amino‐4‐phenylthiazole on platinum electrode in acid medium was carried out under different reaction conditions such as temperature, current density, hydrochloric acid, and monomer concentrations with duration time. The initial rate of the electrocopolymerization reaction on platinum electrode is small and the rate law is Rp = K2 [D]1.29[HCl]0.97[M]1.94. The apparent activation energy is found to be 38.87 kJ/mol. The obtained copolymer film is characterized by 1H‐NMR, elemental analysis, GPC IR, UV‐visible, and cyclic voltammetry and compared with those of the two homopolymers. The mechanism of the electrocopolymerization reaction is also discussed and the monomer reactivity ratio (r1and r2) is calculated. The thermogravimetric analysis (TGA) is used to confirm the proposed structure and determination of the number of water molecules in the polymeric chain unit. X‐ray and scanning electron microscopic analysis are used to investigate the surface morphology. © 2005 Wiley Periodicals, Inc. J Appl Polym Sci 97: 2076–2087, 2005

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.