WO3 and WO3:P (5 mol% H3PO4) thin films were prepared using the sol-gel route and the electrochromic properties of the films were investigated using in situ spectroelectrochemical methods. The measurements were performed in propylene carbonate solution with 0.1 M LiClO4 as electrolyte. During the cathodic polarization at –0.8 V a blue coloration is observed with a reversible variation between 14% and 84% of the transmittance at λ=633 nm. The kinetics for the bleaching process is faster for the WO3:P film than for the undoped WO3 film.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.