Abstract
The Nb-doped WO3 films were deposited by e-beam co-evaporation method using ceramic WO3 targets and metal Nb slugs. The films were analyzed by glancing incident angle X-ray diffraction (GIAXRD), UV/visible spectrophotometer, electrochemical cyclic voltammetry, X-ray photoelectron spectroscopy (XPS). The as-prepared film is brown and amorphous in structure. The film has low transmission in optical visible region. The XPS results indicate that the as-deposited film is non-stoichiometric. By applying a negative potential, the as-deposited film does not show obvious electrochromic effect. However, the electrochromic properties of Nb-doped WO3 films are improved by post annealing treatment at 350, 400, and 450°C in oxygen atmosphere. The Nb-doped WO3 films transform into crystalline structure and become transparent after post annealing treatment. The energy band gap, optical modulation, and color efficiency increase with annealing temperature.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.