A novel electrochemical method for deposition of ZrO(2) thin films is described. The films, 50-600 nm thick, were obtained by applying moderate positive or negative potentials (+2.5 V to -1.5 V versus SHE) on conducting surfaces immersed in a 2-propanol solution of zirconium tetra-n-propoxide [Zr(OPr)(4)] in the presence of minute quantities of water (water/monomer molar ratios in the range of 10(-5) to 10(-1)), which was the limiting reagent. Oxidative electrochemical formation of solvated H(+) and reductive formation of OH(-) catalyze the hydrolysis and condensation of the metal alkoxide precursor. The magnitude of the applied potential and its duration provide a convenient way of controlling the film thickness. The films consist of an amorphous phase, as revealed by XRD measurements. The effects of different parameters, such as the applied potential and its duration, the amount of added water and the current-time characteristics, were studied. A mechanism for the electrodeposition of the zirconia films which is in accordance with our findings is proposed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.