Abstract
The effects of different experimental parameters influencing the determination of critical pitting and protection potentials of aluminium and its alloys are discussed. The simplest mechanical sample preparation, 0.05 mol dm −3 NaCl 1 mol dm −3 Na 2SO 4 test solution, CV polarization with 10-0.1 mV s −1 sweep rate are the suitable experimental conditions. The standard deviation of the characteristic potentials are different; it is less than 5 mV at protection potential and less than 20 mV in the case of pitting potential. The effect of intermetallic phase composition is investigated in a certain range.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.