Abstract

The compositions Li10GeP2S12-x A x (A = O, Se) solid electrolytes were synthesized. As x inreases, the ionic conductivity of the Li10GeP2S12-x O x samples decreases from 2.8 mS/cm to 1.09 mS/cm. Li10GeP2S11.8Se0.2 has the highest ionic conductivity, 3.43 mS/cm, and the activation energy of 0.143 eV. The electrochemical stability is Li10GeP2S11.6O0.4 > Li10GeP2S12 > Li10GeP2S11.8Se0.2, and the electrochemical window of Li10GeP2S11.6O0.4 is about 1.40 – 3.00 V. The difference in electrochemical properties of Li10GeP2S12-x A x (A = O, Se) can be used as a way to improve the interface of Li10GeP2S12-type solid batteries.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.