Carbon-coated lithium iron phosphate (LiFePO 4/C) composites were synthesized by conventional mechanical activation (MA) process and also by a modified MA process. Phase-pure particles were obtained of ∼100 nm size with a nano-meter thick web of carbon surrounding the particles. The composite prepared by the modified MA process shows good performance as cathode material in lithium cells at room temperature. A high performance was achieved at 0.1 C-rate with >96% utilization of the active material. A stable cycle performance even at higher C-rates was achieved with a cathode that has a total carbon content of only 12 wt%. The use of the modified MA process to synthesize LiFePO 4/C has promise to be an efficient process to decrease the total carbon content of the cathode, resulting in the enhanced energy density.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.