Abstract
Abstract An experimental, potential-pH diagram was constructed for the nickel-based Alloy 690 (UNS N06690) in 25°C concentrated (5 M) sodium chloride (NaCl) solution, using an electrochemical hysteresis method. The domains of immunity, general corrosion, passivation, and pitting in 5-M NaCl solutions were defined. At pH > 4, the passive region subdivided into areas of perfect passivation, imperfect passivation, and pitting. After anodic polarization, the surface of each specimen was carefully examined metallographically. Pitting corrosion was observed over the entire pH range investigated (0.3 to 8.52), but general corrosion predominated at lower pH values (<3). On the other hand, the mechanical properties, such as ultimate tensile strength (UTS), strain at fracture, and the reduction area (RA) measured by the slow strain rate test (SSRT), decreased significantly at pH < 3. The SSRT results are consistent with fractography and side-view observations of the tested specimens by scanning electron microscopy (SEM).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.