Abstract

Iron oxide films have been grown on two nickel-chromium-based superalloys, Inconel 600 and 690, by cathodic electrodeposition from an alkaline Fe(III)-Triethanolamine electrolytic solution. The deposition mechanism has been studied by combining thermodynamic calculations, linear sweep voltammetry and the quartz crystal microbalance techniques. Films have been grown at constant potential ranging between −1.01 and −1.30V versus the saturated calomel electrode (SCE). They have been thoroughly characterized by scanning electron microscopy, focused ion beam, magnetometry and X-ray diffraction. Magnetite (Fe3O4) is deposited between −1.01 and −1.09V vs. SCE. Between −1.10 and −1.20V vs. SCE a dual layered structure composed of a dense inner layer and a porous outer thick layer is obtained. These duplex structures are shown to be mainly composed of magnetite and contain some maghemite. Below −1.20V vs.SCE, a dense metallic iron layer is deposited. We have defined experimental protocol parameters to grow dense, highly crystallized, adhesive, magnetite films with controlled thicknesses up 50μm. These magnetite films show a high saturation magnetization of 91.6emug−1 and a small coercivity of 40Oe.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.