AbstractFor a formation of metal hydride of MgH2 or AlH3 under room temperature and ambient pressure, the cathode electrodes of metal and lithium hydride are electrochemically charged with Li anode electrodes in the system of Li-ion extraction. For MgH2 formation, the VC (Voltage-Composition) curve of Mg + 2LiH during charge shows a plateau voltage at 0.6 V until the final composition of 1.05 Li extraction. After charge MgH2 phase is observed by the XRD measurement. Therefore MgH2 is produced by the electrochemical charge from Mg and LiH. For AlH3 formation, Al + 3LiH is charged until the final composition of 0.6 Li at a plateau voltage of 0.8 V which corresponds to the reaction between Al and LiH for the formation of AlH3. In the XRD profile after charge AlH3 phase is not detected although the intensities of Al and LiH decrease compared with these before charge, which suggests the reaction leading to the formation of AlH3.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.