Abstract Three-dimensional macroporous tungsten trioxide (WO3) was electrochemically prepared by using the polystyrene opal as a template. The photonic stop band of the porous WO3 film could be changed when the WO3 was intercalated with lithium cation by the electrochemical method. The change of the stop band was attributed to the change of the refractive indices accompanied with the electrochromism of WO3.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.