Abstract

The fundamental electrochemical properties of the copper-glycine system were investigated in this study to understand the factors that affect the dissolution of metallic copper. Potentiodynamic polarisation measurements were carried out over the pH range 9.0 to 11.5, at temperatures of 22 °C and 60 °C and glycine concentrations 0.1 M and 0.3 M. A window for maximum corrosion current was determined to be between pH 10.0 and 10.5 with a maximum at 60 °C and 0.3 M glycine. Passivation was only observed at pH values >10.5, and then only at potentials above 0.4 V (vs SHE) for quiescent solutions. This passivation potential increased with the rotation speed of the copper electrode. The passive layer broke down after a short rest at the open circuit potential, which allowed reactivation of the surface and high initial currents to briefly flow until the layer re-formed. Potential-step and capacitance measurements are consistent with the formation of a duplex oxide layer of Cu2O and CuO that thickens with increasing potential. The copper glycinate complex itself also acts as an oxidising agent, the effectiveness is increased with its concentration and the concentration of free glycine. Free glycine is oxidised irreversibly above 1.2 V (vs SHE).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.