Abstract

The electrochemical behaviour and corrosion of lead in various concentrations of acetic, lactic (0·01 M–1·0 M), oxalic and tartaric (0·01 M–0·15 M) acid solutions were studied at 25°C by a potentiodynamic method. The lead anode is readily soluble both in acetic and lactic acid solutions up to 2000 mV. In these two acid solutions, the anodic dissolution of lead increases with increases in the acid concentration and the dissolution process is under charge transfer control. Lactic acid is more corrosive than acetic acid. However, in oxalic and tartaric acid solutions, the E/i profiles depend on the acid concentration. Above a certain specific concentration, the profiles exhibit an anodic current peak associated with a dissolution of the metal and the formation of a passivating lead salt film and a cathodic peak which is related to the reduction of the film. The active dissolution of the lead increases with the acid concentration, the scan rate and stirring of the solution. The passivation of lead in these two acid solutions occurs by a dissolution–precipitation mechanism and the process is controlled by diffusion. X-ray diffraction analysis confirmed the presence of a passivating salt film (either lead oxalate or lead tartrate) on the electrode surface. © 1998 SCI

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call