Abstract
The electro-optical properties of the PMN-xPT single-crystal relaxor solid solutions with different PT contents (x = 6, 10, 13%) and the PLMN-25PT transparent ceramic with a La content of 3%, which has been synthesized for the first time, have been studied at room temperature. It has been shown that the dependence of the quadratic electro-optical coefficients on the PT concentration in single crystals passes through a maximum at x ∼ 13%. It has been revealed that, although the PT concentration in the PLMN-25PT ceramic is above 13%, this material exhibits the largest quadratic electro-optical coefficients and the lowest half-wave voltage among all the known relaxor systems. Possible origins of the above phenomena have been discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.