Abstract
Specific heat and electrical resistivity were measured on La 2−X Sr X NiO 4+δ with various Sr concentrations as a function of temerature. The behaviors of electrical resistivity and lattice constants show a marked change at X⋃0.5 (Xc). The specific heat shows a hump at about 6K in C/T vs. T 2 plot for all of samples annealed in air. For the samples annealed in hydrogen no hump is observed. The relationship between Xc and interstitial oxygen defect is discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.