Ga2O3 and Ga2O3-TiO2 (GTO) nano-mixed thin films were prepared by plasma enhanced atomic layer deposition with an alternating supply of reactant sources, [(CH3)2GaNH2]3, Ti(N(CH3)2)4 and oxygen plasma. The uniform and smooth Ga2O3 and GTO thin films were successfully deposited. Excellent step coverage of these films was obtained by chemisorbed chemical reactions with oxygen plasma on the surface. The dielectric constant of GTO thin film definitely increased compared to Ga2O3 film, and the leakage currents of GTO films were comparable to Ga2O3 films. The leakage current density of a 40-nm-GTO film annealed at 600∘C was approximately 1×10−7 A/cm2 up to about 600 kV/cm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.