Abstract
Thin films of calcium-strontium bismuth titanate (Ca1-xSrx)Bi4Ti4O15 solid solution were fabricated on (111)Pt/Ti/SiO2/(100)Si substrates by a chemical-solution deposition (CSD) technique. These films had x = 0–1.00 and consisted of a polycrystalline structure with random orientation of the bismuth layer-structured ferroelectric (BLSF) crystal (m = 4). The relative dielectric constants of (Ca1-xSrx)Bi4Ti4O15 films were enhanced from 40 to 220 with increasing x; these values did not vary significantly with changes in the measuring frequency and the bias field. The temperature coefficient of the relative dielectric constant at around room temperature became larger with increasing x from 0 to 1.00; the change in the dielectric constant of these film between 30–100°C increased from 2% to 15%.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.