Abstract
PCO (Praseodymium Cerium Oxide) solid solution (0-50% PrOx) has been prepared by the conventional solid-state ceramic processing of mixed CeO2 and PrOx powders in the desired stoichiometry at 1500°C in air. Synthesized powder has been characterized for phase chemistry and lattice structure. Electrochemical characteristics of the synthesized powder has been examined using electrochemical impedance spectroscopy. The observed increase in the electrical conductivity of PCO are associated with increased concentration of oxygen vacancies created by replacement of Ce4+ ions with Pr+3 ions. The addition of PrOx also lowered the polarization and ohmic losses.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.