Abstract

A significant improvement of contact transfer resistance on undoped GaN/AlGaN/AlN (10 Å)/ GaN high electron mobility transistor (HEMT) structure was demonstrated using a Ta/Ti/Al/Mo/Au metallization scheme compared to a Ti/Al/Mo/Au metallization scheme. A contact resistance as low as 0.16 ± 0.03 ohm - mm was achieved by rapid thermal annealing of evaporated Ta (125 Å)/ Ti (150 Å)/ Al (900 Å)/ Mo (400 Å)/ Au (500 Å) metal contact at 700 °C for 1 min followed by 800 °C for 30 sec in a N 2 ambient. An excellent edge acuity was also demonstrated for the annealed Ta/Ti/Al/Mo/Au ohmic contacts.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.