Processes of the polarization switching in ceramic relaxors Pb(Mg1/3Ti1/3W1/3)O3, Pb(Mg1/4Sc1/4Nb1/4W1/4)O3, Pb(Mg1/5Sc1/5Ti1/5Nb1/5W1/5)O3, and Pb(Mg1/6Sc1/6Ti1/6Sn1/6Ta1/6W1/6)O3 have been investigated at frequencies from 50 Hz to 2 kHz in the temperature range 90–300 K for measuring field amplitudes up to 20 kV/cm. It has been demonstrated that, under specific conditions, these materials are characterized by saturated dielectric hysteresis loops, which indicate the appearance of the ferroelectric state induced by the electric field. The dependences of the spontaneous polarization and the coercive field of the relaxors under investigation on their chemical composition, temperature, and frequency of the measuring voltage have been determined.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.