Abstract
Abstract Applied field dependence of static dielectric constant, and also dc bias field dependence of high frequency dielectric constant from 1 MHz to 100 MHz are measured in the helicoidal smectic C phase of ferroelectric liquid crystal (+)DOBAMBC. A very low characteristic threshold field, which may be thought as a coerceive field of Goldstone mode, E = 3.8 × 10−3 V/cm (at 82°C) was found in the static dielectric constant measurement by lock in amp and thermal noise method. The high frequency dielectric constant is temperature independent above from 10 MHz. A lucid ⊊ -E hysteresis loop by dc bias field E and its critical behaviour in 50 MHz region are observed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.